Inconel 718

Inconel 718 | Inconel Alloy 718 | Nickel Alloy | Seamless Tubes Inconel Alloy | Inconel Alloy Manufacturers | Manufacturer of Nickel Alloy Manufacturer of Inconel Alloy | Inconel Alloy 718 | Inconel Alloy 718 Exporters | Inconel Alloy 07718 | UNS 07718 | Inconel Alloy Manufacturer Near You | Inconel Alloy | Inconel Alloy Supplier | Exporter of Inconel Alloy

Overview:

Namah Super Alloys is a trusted manufacturer, supplier, stockist, and exporter of premium Nickel Alloy and High-Performance Alloy products. With a commitment to quality and precision, we specialize in a wide range of products including Rods (Bright Bars), Sheets & Plates, Pipes & Tubes, Pipe Fittings (Flanges, Elbows, Tees, Reducers, Nipples, etc.), Fasteners (Nuts, Bolts, Studs), CNC Components, and Sheet, Plate & Coils.

Our materials are renowned for their exceptional strength, corrosion resistance, and thermal stability, making them suitable for critical applications across industries such as aerospace, oil & gas, petrochemicals, marine, power generation, and defense. We offer custom and standard sizes, ensuring optimal performance in both high-pressure and corrosive environments. With superior machinability, weldability, and dimensional accuracy, Namah Super Alloys delivers components that meet the most demanding international standards and client specifications.

Alloy 718 is a nickel-chromium alloy with additions of niobium & molybdenum which can be heat-treated to give high strength, good corrosion resistance, ease of formability and which can be welded with good resistance to strain age cracking. The alloy can be used at temperatures up to 700ºC.

Alloy 718 for the oil industry is heat treated such that the hardness does not exceed 40HRC which is the maximum allowed by NACE MR-01-75/ ISO 15156: 3 to prevent stress corrosion cracking. The major applications in this field are Valves and precision tubing.

Alloy 718 for aerospace and power generation is heat treated to give maximum strength and high creep resistance with typical hardness values exceeding 42HRC. The major applications are components for gas turbines, aircraft engines, fasteners and other high strength applications.

AVAILABLE TUBE PRODUCT FORMS
Straight Tube | Straight Pipe | U - Tube | Coiled Tube
TYPICAL MANUFACTURING SPECIFICATIONS
ASME SB-161 ASTM B622/ASME SB622
ASME SB-163 ASTM B725/ASME SB725
ASME SB-775 ASTM B829/ASME SB829
TYPICAL APPLICATIONS
HEAT EXCHANGERS
WELL HEAD COMPLETION EQUIPMENT
MANDRELS
VALVES
INDUSTRIES PREDOMINANTLY USING THIS GRADE
AEROSPACE
OIL AND GAS
NUCLEAR AND POWER

Typical Specification

CHEMICAL COMPOSITION (% by weight)
Element C Si Mn P Al B Co Cr Cu Fe Mo Nb Ni Ti
Min - - - - 0.2 - - 17 - Balance 2.8 4.75 50 0.65
Max 0.08 0.35 0.35 0.015 0.8 0.60 1 21 0.3 Balance 3.3 5.5 55 1.15
PHYSICAL PROPERTIES (Room Temperature)
Specific Heat (0-100°C) 435 J.kg-1.°K-1
Thermal Conductivity 11.4 W.m -1.°K-1
Thermal Expansion 13 mm/m/°C
Modulus Elasticity 200 GPa
Electrical Resistivity 1.32 Ohm-cm
Density 8.19 g/cm3
MECHANICAL PROPERTIES
Temper Annealed
Tensile Rm 155 ksi (min)
Tensile Rm 1069 MPa (min)
R.p. 0.2% Yield 95 ksi (min)
R.p. 0.2% Yield 655 MPa (min)
Elongation (2” or 4D gl) 30 % (min)
Cart
  • Your cart is empty Browse Shop
    Select the fields to be shown. Others will be hidden. Drag and drop to rearrange the order.
    • Image
    • SKU
    • Rating
    • Price
    • Stock
    • Availability
    • Add to cart
    • Description
    • Content
    • Weight
    • Dimensions
    • Additional information
    Click outside to hide the comparison bar
    Compare