| Outside Diameter | Birmingham Wire Gauge (BWG) | ||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|
| 20 (0.889 mm) |
18 (1.245 mm) |
16 (1.651 mm) |
15 (1.829 mm) |
14 (2.108 mm) |
13 (2.413 mm) |
12 (2.769 mm) |
11 (3.048 mm) |
10 (3.403 mm) |
|||
| in | mm | Weight, kg/m (average wall') | |||||||||
| 1/4 | 0.250 | 6.350 | 0.12 | 0.16 | 0.19 | - | - | - | - | - | - |
| 5/16 | 0.313 | 7.950 | 0.15 | 0.21 | 0.25 | 0.28 | - | - | - | - | - |
| 3/8 | 0.375 | 9.525 | 0.19 | 0.25 | 0.31 | 0.34 | 0.39 | - | - | - | - |
| 1/2 | 0.500 | 12.700 | 0.25 | 0.34 | 0.45 | 0.49 | 0.55 | 0.61 | 0.68 | 0.72 | - |
| 5/8 | 0.625 | 15.875 | 0.33 | 0.45 | 0.58 | 0.64 | 0.71 | 0.80 | 0.89 | 0.97 | - |
| 3/4 | 0.750 | 19.050 | 0.40 | 0.55 | 0.72 | 0.77 | 0.88 | 0.98 | 1.12 | 1.20 | 1.31 |
| 7/8 | 0.875 | 22.225 | 0.46 | 0.64 | 0.83 | 0.92 | 1.04 | 1.18 | 1.32 | 1.44 | 1.58 |
| 1 | 1.000 | 25.400 | 0.54 | 0.74 | 0.97 | 1.06 | 1.21 | 1.37 | 1.55 | 1.68 | 1.92 |
| 1 1/8 | 1.125 | 28.575 | 0.61 | 0.83 | 1.10 | 1.21 | 1.37 | 1.56 | 1.76 | 1.92 | 2.11 |
| 1 1/4 | 1.250 | 31.750 | 0.68 | 0.94 | 1.23 | 1.35 | 1.53 | 1.76 | 1.96 | 2.16 | 2.40 |
| 1 3/8 | 1.375 | 34.925 | 0.74 | 1.03 | 1.35 | 1.49 | 1.70 | 1.93 | 2.19 | 2.40 | 2.65 |
| 1 1/2 | 1.500 | 38.100 | 0.82 | 1.13 | 1.49 | 1.64 | 1.87 | 2.17 | 2.40 | 2.63 | 2.92 |
| 1 3/4 | 1.750 | 44.450 | 0.97 | 1.32 | 1.74 | 1.92 | 2.20 | 2.50 | 2.84 | 3.10 | 3.44 |
| 2 | 2.000 | 50.800 | - | 1.52 | 1.99 | 2.20 | 2.53 | 2.89 | 3.27 | 3.59 | 3.97 |
| 2 1/4 | 2.250 | 57.150 | - | 1.73 | 2.26 | 2.48 | 2.87 | 3.26 | 3.70 | 4.06 | 4.51 |
| 2 3/8 | 2.375 | 60.325 | - | 1.81 | 2.38 | 2.63 | 3.02 | 3.44 | 3.93 | 4.30 | 4.78 |
| 2 1/2 | 2.500 | 63.500 | - | 1.91 | 2.52 | 2.78 | 3.18 | 3.66 | 4.14 | 4.54 | 5.04 |
| 2 7/8 | 2.875 | 73.025 | - | 2.20 | 2.90 | 3.20 | 3.68 | 4.20 | 4.79 | 5.25 | 5.83 |
| 3 | 3.000 | 76.200 | - | 2.31 | 3.04 | 3.35 | 3.85 | 4.39 | 5.00 | 5.49 | 6.10 |
| 3 1/2 | 3.500 | 88.900 | - | 2.69 | 3.56 | 3.93 | 4.51 | 5.15 | 5.86 | 6.44 | 7.17 |
| 4 | 4.000 | 101.60 | - | - | 4.11 | 4.54 | 5.21 | 5.95 | 6.80 | 7.47 | 8.30 |