Inconel 625 | Nickel Alloy | Seamless Tubes Inconel Alloy | Inconel Alloy Manufacturers | Manufacturer of Nickel Alloy Manufacturer of Inconel Alloy | Inconel Alloy 625 | Inconel Alloy 625 Exporters | Inconel Alloy 06625 | UNS 06625 | Inconel Alloy Manufacturer Near You | Inconel Alloy | Inconel Alloy Supplier | Exporter of Inconel Alloy

Overview:

Namah Super Alloys is a trusted manufacturer, supplier, stockist, and exporter of premium Nickel Alloy and High-Performance Alloy products. With a commitment to quality and precision, we specialize in a wide range of products including Rods (Bright Bars), Sheets & Plates, Pipes & Tubes, Pipe Fittings (Flanges, Elbows, Tees, Reducers, Nipples, etc.), Fasteners (Nuts, Bolts, Studs), CNC Components, and Sheet, Plate & Coils.

Our materials are renowned for their exceptional strength, corrosion resistance, and thermal stability, making them suitable for critical applications across industries such as aerospace, oil & gas, petrochemicals, marine, power generation, and defense. We offer custom and standard sizes, ensuring optimal performance in both high-pressure and corrosive environments. With superior machinability, weldability, and dimensional accuracy, Namah Super Alloys delivers components that meet the most demanding international standards and client specifications.

Alloy 625 is a nickel-chromium-molybdenum alloy used for its high strength, excellent fabricability and outstanding corrosion resistance. Service temperatures can range from cryogenic to 980°C (1800°F). Alloy 625 strength is derived from the solid solution strengthening effect of molybdenum and niobium on its nickel-chromium matrix.

Thus, precipitation-hardening treatments are not required. This combination of elements is also responsible for superior resistance to a wide range of corrosive environments of unusual severity, as well as to high-temperature effects such as oxidation and carburization.

AVAILABLE TUBE PRODUCT FORMS
Straight Tube | Straight Pipe | U - Tube | Coiled Tube
TYPICAL MANUFACTURING SPECIFICATIONS
ASME SB-161 ASTM B622/ASME SB622
ASME SB-163 ASTM B725/ASME SB725
ASME SB-775 ASTM B829/ASME SB829
TYPICAL APPLICATIONS
WELLHEAD COMPONENTS
SHEATHING
DOWNHOLE EQUIPMENT FOR CORROSIVE / SOUR SERVICE
REACTOR CORE
CONTROL ROD COMPONENTS
GAS PIPELINE CONTROL LINES
HEAT EXCHANGERS
OIL REFINING
CHEMICAL PROCESSING
CONTROL AND INSTRUMENTATION TUBES
INDUSTRIES PREDOMINANTLY USING THIS GRADE
CHEMICAL PROCESSES
OIL AND GAS
NUCLEAR AND POWER

Typical Specification

Element C Si Mn P S Al Cr Fe Mo Nb Ni Ti
Min - - - - - - 20 - 8 3.150 Balance -
Max 0.1 0.5 0.5 0.015 0.015 0.4 23 5 10 4.150 Balance 0.40
PHYSICAL PROPERTIES (Room Temperature)
Specific Heat (0-100°C) 460 J.kg-1.°K-1
Thermal Conductivity 14.8 W.m -1.°K-1
Thermal Expansion 12.4 mm/m/°C
Modulus Elasticity 207 GPa
Electrical Resistivity 10.3 Ohm-cm
Density 8.42 g/cm3
MECHANICAL PROPERTIES
Temper Annealed (Grade 1) Solution-annealed (Grade 2)
Tensile Rm 120 ksi (min) 100 ksi (min)
Tensile Rm 827 MPa (min) 690 MPa (min)
R.p. 0.2% Yield 60 ksi (min) 40 ksi (min)
R.p. 0.2% Yield 414 MPa (min) 276 MPa (min)
Elongation (2” or 4D gl) 30 % (min) 30 % (min)
Cart
  • Your cart is empty Browse Shop
    Select the fields to be shown. Others will be hidden. Drag and drop to rearrange the order.
    • Image
    • SKU
    • Rating
    • Price
    • Stock
    • Availability
    • Add to cart
    • Description
    • Content
    • Weight
    • Dimensions
    • Additional information
    Click outside to hide the comparison bar
    Compare