Hastelloy C-276

Hastelloy C 276 | Inconel Alloy 276 | Nickel Alloy | Seamless Tubes Inconel Alloy | Inconel Alloy Manufacturers | Manufacturer of Nickel Alloy Manufacturer of Inconel Alloy | Inconel Alloy 276 | Inconel Alloy 276 Exporters | Inconel Alloy 10276 | UNS 10276 | Inconel Alloy Manufacturer Near You | Inconel Alloy | Inconel Alloy Supplier | Exporter of Inconel Alloy

Overview:

Namah Super Alloys is a trusted manufacturer, supplier, stockist, and exporter of premium Nickel Alloy and High-Performance Alloy products. With a commitment to quality and precision, we specialize in a wide range of products including Rods (Bright Bars), Sheets & Plates, Pipes & Tubes, Pipe Fittings (Flanges, Elbows, Tees, Reducers, Nipples, etc.), Fasteners (Nuts, Bolts, Studs), CNC Components, and Sheet, Plate & Coils.

Our materials are renowned for their exceptional strength, corrosion resistance, and thermal stability, making them suitable for critical applications across industries such as aerospace, oil & gas, petrochemicals, marine, power generation, and defense. We offer custom and standard sizes, ensuring optimal performance in both high-pressure and corrosive environments. With superior machinability, weldability, and dimensional accuracy, Namah Super Alloys delivers components that meet the most demanding international standards and client specifications.

Alloy 276 is a nickel-molybdenum-chromium superalloy with an addition of tungsten designed to have excellent corrosion resistance in a wide range of severe environments. The high chromium, molybdenum and tungsten contents make the alloy especially resistant to pitting and crevice corrosion in reducing environments while chromium conveys resistance to oxidizing media. The low carbon content minimizes carbide precipitation during welding to maintain corrosion resistance in as-welded structures.

This nickel alloy is resistant to the formation of grain boundary precipitates in the weld heat-affected zone, thus making it suitable for most chemical process application in an as welded condition. Alloy 276 is widely used in the most severe environments such as mixed acid chemical processing, pollution control, pulp and paper production, industrial and municipal waste treatment, and recovery of sour oil and gas.

AVAILABLE TUBE PRODUCT FORMS
Straight Tube | Straight Pipe | U - Tube | Coiled Tube
TYPICAL MANUFACTURING SPECIFICATIONS
ASME SB-161 ASTM B622/ASME SB622
ASME SB-163 ASTM B725/ASME SB725
ASME SB-775 ASTM B829/ASME SB829
TYPICAL APPLICATIONS
POLLUTION CONTROL
MIXED ACID CHEMICALS
PULP AND PAPER PRODUCTION S
WASTE TREATMENT
VERY HIGH CHLORIDE ENVIRONMENTS
INDUSTRIES PREDOMINANTLY USING THIS GRADE
CHEMICAL PROCESSES
OIL AND GAS

Typical Specification

CHEMICAL COMPOSITION (% by weight)
Element C Si Mn P S Co Fe Cr Cu Mo V Ni
Min - - - - - - 4 14.5 3 15 - Balance
Max 0.02 0.08 1 0.030 0.30 2.5 7 16.5 4.5 17 0.35
PHYSICAL PROPERTIES (Room Temperature)
Specific Heat (0-100°C) 427 J.kg-1.°K-1
Thermal Conductivity 9.4 W.m -1.°K-1
Thermal Expansion 11.2 mm/m/°C
Modulus Elasticity 221 GPa
Electrical Resistivity 1.30 Ohm-cm
Density 8.89 g/cm3
MECHANICAL PROPERTIES
Temper Annealed
Tensile Rm 100 ksi (min)
Tensile Rm 690 MPa (min)
R.p. 0.2% Yield 41 ksi (min)
R.p. 0.2% Yield 290 MPa (min)
Elongation (2” or 4D gl) 40 % (min)
Cart
  • Your cart is empty Browse Shop
    Select the fields to be shown. Others will be hidden. Drag and drop to rearrange the order.
    • Image
    • SKU
    • Rating
    • Price
    • Stock
    • Availability
    • Add to cart
    • Description
    • Content
    • Weight
    • Dimensions
    • Additional information
    Click outside to hide the comparison bar
    Compare