Inconel 600

Inconel 600 | Seamless Tubes Inconel Alloy | Inconel Alloy Manufacturers Manufacturer of Inconel Alloy | Inconel Alloy 600 | Inconel Alloy 600 Exporters | Inconel Alloy Manufacturer Near You | Inconel Alloy | Inconel Alloy Supplier | Exporter of Inconel Alloy

Overview:

Namah Super Alloys is a trusted manufacturer, supplier, stockist, and exporter of premium Nickel Alloy and High-Performance Alloy products. With a commitment to quality and precision, we specialize in a wide range of products including Rods (Bright Bars), Sheets & Plates, Pipes & Tubes, Pipe Fittings (Flanges, Elbows, Tees, Reducers, Nipples, etc.), Fasteners (Nuts, Bolts, Studs), CNC Components, and Sheet, Plate & Coils.

Our materials are renowned for their exceptional strength, corrosion resistance, and thermal stability, making them suitable for critical applications across industries such as aerospace, oil & gas, petrochemicals, marine, power generation, and defense. We offer custom and standard sizes, ensuring optimal performance in both high-pressure and corrosive environments. With superior machinability, weldability, and dimensional accuracy, Namah Super Alloys delivers components that meet the most demanding international standards and client specifications.

Alloy 600 is a nickel-chromium alloy designed for use from cryogenic to elevated temperatures in the range of 2000°F (1093°C). The high nickel content of the alloy enables it to retain considerable resistance under reducing conditions and makes it resistant to corrosion by a number of organic and inorganic compounds. The nickel content gives it excellent resistance to chloride-ion stress-corrosion cracking and also provides excellent resistance to alkaline solutions.

Its chromium content gives the alloy resistance to sulphur compounds and various oxidizing environments. The chromium content of the alloy makes it superior to commercially pure nickel under oxidizing conditions. In strong oxidizing solutions like hot, concentrated nitric acid Alloy 600 has poor resistance. Alloy 600 is relatively un-attacked by the majority of neutral and alkaline salt solutions and is used in some caustic environments. The alloy resists steam and mixtures of steam, air and carbon dioxide.

AVAILABLE TUBE PRODUCT FORMS
Straight Tube | Straight Pipe | U - Tube | Coiled Tube
TYPICAL MANUFACTURING SPECIFICATIONS
ASME SB-161 ASTM B622/ASME SB622
ASME SB-163 ASTM B725/ASME SB725
ASME SB-775 ASTM B829/ASME SB829
TYPICAL APPLICATIONS
HEAT EXCHANGERS
THERMOCOUPLES
CONTROL AND INSTRUMENTATION TUBES
INDUSTRIES PREDOMINANTLY USING THIS GRADE
CHEMICAL PROCESSES
NUCLEAR AND POWER

Typical Specification

CHEMICAL COMPOSITION (% by weight)
Element C Si Mn S Cr Cu Fe Ni
Min - - - - 14 - 6 72
Max 0.15 0.5 1 0.015 17 0.5 10 -
PHYSICAL PROPERTIES (Room Temperature)
Specific Heat (0-100°C) 460 J.kg-1.°K-1
Thermal Conductivity 14.8 W.m -1.°K-1
Thermal Expansion 13.9 mm/m/°C
Modulus Elasticity 173 GPa
Electrical Resistivity 5.47 Ohm-cm
Density 8.83 g/cm3
MECHANICAL PROPERTIES
Temper Annealed
Tensile Rm 110 ksi (min)
Tensile Rm 738 MPa (min)
R.p. 0.2% Yield 37 ksi (min)
R.p. 0.2% Yield 255 MPa (min)
Elongation (2” or 4D gl) 45 % (min)
Cart
  • Your cart is empty Browse Shop
    Select the fields to be shown. Others will be hidden. Drag and drop to rearrange the order.
    • Image
    • SKU
    • Rating
    • Price
    • Stock
    • Availability
    • Add to cart
    • Description
    • Content
    • Weight
    • Dimensions
    • Additional information
    Click outside to hide the comparison bar
    Compare