Alloy 20

Incoloy 8020 | Incoloy Alloy | Seamless Tubes Nickel Alloy | Incoloy Alloy 20 Manufacturer | Manufacturer of Nickel Alloy Manufacturer of Nickel Alloy Products | Nickel Incoloy Alloy 20 | Nickel Alloy 8020 Exporters | Nickel Alloy 08020 | UNS N08020 | Incoloy Alloy Manufacturer Near You | Nickel Alloy | Nickel Alloy Supplier | Exporter of Nickel Alloy | Incoloy Alloy Supplier | Exporter of Incoloy Alloy

Overview:

Namah Super Alloys is a trusted manufacturer, supplier, stockist, and exporter of premium Nickel Alloy and High-Performance Alloy products. With a commitment to quality and precision, we specialize in a wide range of products including Rods (Bright Bars), Sheets & Plates, Pipes & Tubes, Pipe Fittings (Flanges, Elbows, Tees, Reducers, Nipples, etc.), Fasteners (Nuts, Bolts, Studs), CNC Components, and Sheet, Plate & Coils.

Our materials are renowned for their exceptional strength, corrosion resistance, and thermal stability, making them suitable for critical applications across industries such as aerospace, oil & gas, petrochemicals, marine, power generation, and defense. We offer custom and standard sizes, ensuring optimal performance in both high-pressure and corrosive environments. With superior machinability, weldability, and dimensional accuracy, Namah Super Alloys delivers components that meet the most demanding international standards and client specifications.

INCOLOY® alloy 020 (UNS N08020) has excellent corrosion resistance in chemical environments containing sulfuric acid, and useful resistance to environments containing chlorides, nitric acid, and phosphoric acid. Other uses include the production of gasoline, solvents, explosives, inorganic and organic chemicals, pharmaceuticals, and food and synthetic materials. INCOLOY alloy 020 is readily fabricated to produce mixing tanks, heat exchangers, process piping, pickling equipment, pumps, valves, fasteners and fittings. Applications for alloy 020 requiring resistance to aqueous corrosion are essentially the same as those for INCOLOY alloy 825.

A nickel-iron-chromium alloy with additions of copper and molybdenum. It also contains niobium for stabilization against sensitization and resultant intergranular corrosion. The alloy has excellent resistance to general corrosion, pitting and crevice corrosion in chemicals containing chlorides and sulfuric, phosphoric and nitric acids. Used for tanks, piping, heat exchangers, pumps, valves and other process equipment.

AVAILABLE TUBE PRODUCT FORMS
Straight Tube | Straight Pipe | U - Tube | Coiled Tube
TYPICAL MANUFACTURING SPECIFICATIONS
ASME SB-161 ASTM B622/ASME SB622
ASME SB-163 ASTM B725/ASME SB725
ASME SB-775 ASTM B829/ASME SB829
TYPICAL APPLICATIONS
HEAT EXCHANGERS
WELL HEAD COMPLETION EQUIPMENT
MANDRELS
VALVES
INDUSTRIES PREDOMINANTLY USING THIS GRADE
AEROSPACE
OIL AND GAS
NUCLEAR AND POWER

Typical Specification

CHEMICAL COMPOSITION (% by weight)
Element Ni Nb + Ta Mn Mo P Cr Nb S Cu C Si Fe
Min 32 8xC - 2.0 - 19.0 - - 3.0 - - Balance
Max 38 1.0 2.0 3.0 0.045 21.0 1.0 0.035 4.0 0.07 1.0 Balance
PHYSICAL PROPERTIES (Room Temperature)
Specific Heat 0.12 Btu/lb•°F 500 J/kg•°C
Coefficient of Expansion 8.2 77 – 212°F, 10-6 in/in•°F 14.7 25 – 100°C, µm/m•°C
Thermal Conductivity 85 Btu • in/ft2 •h•°F 12.3 W/m • °C
Electrical Resistivity 651 ohm • circ mil/ft 1.08 µΩ•m
Density 0.292 Ib/in3 8.08 g/cm3
MECHANICAL PROPERTIES
Temper Annealed
Tensile Strength 90 ksi (min)
Tensile Strength 620 MPa (min)
R.p. 0.2% Yield 45 ksi (min)
R.p. 0.2% Yield 300 MPa (min)
Elongation (2” or 4D gl) 40 % (min)
Cart
  • Your cart is empty Browse Shop
    Select the fields to be shown. Others will be hidden. Drag and drop to rearrange the order.
    • Image
    • SKU
    • Rating
    • Price
    • Stock
    • Availability
    • Add to cart
    • Description
    • Content
    • Weight
    • Dimensions
    • Additional information
    Click outside to hide the comparison bar
    Compare